What are the results of high indoor relative humidity?
Possible solutions? - Results:
- Mould growth
- Poor indoor air quality
Solutions:
- Ventilation
- Dehumidification
- Bufering (buffer material taking up water)
What are results of capillary rise?
What are possible solutions - Results:
,- salt efflorescence
- rendering degradation
- poor indoor air quality
Solutions:
- liquid water barrier
- enhanced drying by ventilation
What are results of leakage? - - cracking
- salt efflorescence
Name different degradation mechanisms - Mechanisms:
- physical
- chemical
- biological
--> coupled, interacting
What is one of the main reasons for construction problems related to degradation? -
Moisture
Water triggers physical, chemical and biological processes!
(Estimate: 70% of all problems related to moisture)
When does physical degradation occur? - When the material can no longer sustain the
loads it is exposed to
(Loads due to
- mechanical loading
- hygric loading
- thermal loading
- ...)
Name different types of mechanical sstress that can lead to physical degradation. - -
snow load
- ponding
- moisture load
What is hygric stress? - Material deformation:
- drying shrinkage
- swelling during wetting
--> can cause failure when
- deformation is limited (cracking/ buckling)
- internal stress > material strength
, What are solutions when restrained shrinkage occurs in an outside render? - applied on
wet wall:
-> wait until wall is dry
-> reinforce render
applied on dry wall:
-> reinforce render
What is thermal stress?
Solution? - Material expansion from heat
-> potential buckling/cracking when restrained
Solution: Provide space (tolerance) for expansion
What is crystallization stress? - freeze/thaw (frost) damage
-> liquid water freezes and expands (+9% in volume)
-> stress in limited pore volume
-> material failure if stress > material strength
Describe 3 types of crystallization stress - 1. Frost scaling
- water film on surface
- freezing of film
- ice contracting if cooling continues
- cracking of film --> propagates into material underneath
2. salt weathering
- material with initial cracks wetted with saline water
- water evaporates, salt crystallizes
- crystals expand, crack -> propagates into material
3. salt efflorescence
- crystallinsing not in material, but on surface
- damage mainly aesthetical
Describe 2 types of chemical degradation. - 1. corrosion (of reinforcement)
- rust occupies more volume than iron -> iron expansion in concrete
- induces mechanical stress -> cracking/spalling
2. leaching
- wetting of material with initial cracks /open porosity
- dissultion of minerals in material
Voordelen van het kopen van samenvattingen bij Stuvia op een rij:
Verzekerd van kwaliteit door reviews
Stuvia-klanten hebben meer dan 700.000 samenvattingen beoordeeld. Zo weet je zeker dat je de beste documenten koopt!
Snel en makkelijk kopen
Je betaalt supersnel en eenmalig met iDeal, creditcard of Stuvia-tegoed voor de samenvatting. Zonder lidmaatschap.
Focus op de essentie
Samenvattingen worden geschreven voor en door anderen. Daarom zijn de samenvattingen altijd betrouwbaar en actueel. Zo kom je snel tot de kern!
Veelgestelde vragen
Wat krijg ik als ik dit document koop?
Je krijgt een PDF, die direct beschikbaar is na je aankoop. Het gekochte document is altijd, overal en oneindig toegankelijk via je profiel.
Tevredenheidsgarantie: hoe werkt dat?
Onze tevredenheidsgarantie zorgt ervoor dat je altijd een studiedocument vindt dat goed bij je past. Je vult een formulier in en onze klantenservice regelt de rest.
Van wie koop ik deze samenvatting?
Stuvia is een marktplaats, je koop dit document dus niet van ons, maar van verkoper VasilyKichigin. Stuvia faciliteert de betaling aan de verkoper.
Zit ik meteen vast aan een abonnement?
Nee, je koopt alleen deze samenvatting voor €12,88. Je zit daarna nergens aan vast.